FYI, if you indeed used plumber's flux, you have to clean the board with WATER. And very well. The zinc chloride and other salts left behind will not dissolve in break cleaner. It is possible to use plumber's flux on copper/tin electrical connections, but it is a pain to remove the flux, sufficiently. You cannot use it on steel/iron, though. You will never remove all of the salts, and the connection WILL definitely corrode over time, because the acid creates tiny pores in the iron where the salts get imbedded.
Certain no clean fluxes will also leave a slightly conductive residue, especially when used incorrectly.
Rosin flux, you should be cake. I use MG 835, and it's fine. RA flux is sorta well specified. The military came up with specifications for R, RMA, and RA. Anywhere you buy it, it is essentially the same. (This is one reason why flux manufacturers spend so much time coming up with better mousetraps.... they can only charge as much for rosin flux as the next guy; hence, margin on it is relatively small).
So your circuit might be salvageable. I don't know what the brake cleaner did to it. But I would try hot water and a toothbrush before disposing of it. That said, I dunno if you really used plumber's flux. The jar says acid-free. Around here, anyway, "plumber's flux" means zinc chloride. And this creates hydrochloric acid when heated.