If you are going to etch regularly, consider cupric chloride:
http://jimlaurwilliams.org/projects/seychellePaper/index.htmlIn a nutshell, this starts with your typical HCl+H2O2 method, but instead of throwing it away, you just keep accumulating the "waste", and the "waste" itself slowly starts becoming useful! You add less and less H2O2, until the cupric chloride concentration in your solution is high enough to work on its own, and no H2O2 is needed anymore. What's left is adding a tiny little bit of HCl every now and then; the consumption is down to maybe 1/20 to 1/50 what it is on a single-use HCl+H2O2 method.
You still need to consider the fume handling.
Strong bubbling is very much recommended - not only to speed up etching, and not only for the self-regeneration process; but also to increase the etching resolution.
In H2O2 single use non-bubbled quick etching, I always found practical line width limit at around 10 mils on 1oz clad, whereas a strongly bubbled bath can do 8 mils on 1oz clad very easily and robustly, and 6 mils on 0.5oz.
Strong bubbling, though, generates even more acid mist, so I'd do it outdoors or design a proper fume hood.
We have used this process since... 2012? .. in a club enviroment where a lot of PCBs get done. About a litre of HCl needs to be added only about once a year, which is great because someone needs to get the acid and maintain the process, and this is the only process that runs almost unmaintained! At some point, no one added any HCl for about two years, and the process slowed down from the usual 12 minutes to about 25 minutes, but was still usable.
We built our tank out of PVC (by gluing, using specific PVC glue designed to build tanks), which holds about 6-8 liters of etchant, with a big bubbler on the bottom (also made of PVC sheets, with small holes drilled all over). We run the bubbler out of compressed air line through a pressure regulator valve. The PCB is held in the lid construction: the lid has a piece of PVC sheet with a bit-less-than 1.6mm gap in it; the PCB sits firmly in the gap, and is held vertically. (Air bubbling tries to force the PCB one way or another, so mounting it firmly is important.)